Why Weld Quality Is Critical in Tanker Manufacturing

December 20, 20254 min readTank Dünyası
Why Weld Quality Is Critical in Tanker Manufacturing

The Weld Is Not the Weakest Link

In a tanker body the most discussed subject is plate thickness. What actually determines leak tightness, strength and life is not the thickness but how the joints are made. A weld seam is the only linear discontinuity in the continuity of the body, so it is both the source of stress concentration and the starting point of corrosion. Weld quality is therefore the primary factor in the life of a tanker.

1. TIG (141) versus MAG (135)

Both methods are numbered to ISO 4063: TIG 141 (GTAW) uses a tungsten electrode in argon shielding, while MAG 135 (GMAW) uses a wire electrode with shielding gas. The choice follows the material and the seam geometry.

Where is which used?

  • Stainless body (AISI 304): TIG 141; argon shielding minimises the risk of carbon steel contamination
  • Carbon steel body (A3 / S235JR): MAG 135; higher travel speed and deposition make it economical on large ring seams
  • Aluminium body: TIG 141; since aluminium is harder to weld, strict cleaning and correct gas flow are essential
  • Attachments: either method may be used; here material compatibility is less decisive than the welding position

The choice of welding method is not a preference but a result dictated by material and position. Two methods may be used on the same body; what matters is that each of them is covered by its own WPS.

2. EN ISO 15614-1: WPS, PQR and WPQR

Weld quality can only be measured if it is documented. The WPS (Welding Procedure Specification) states how a welding operation is to be performed; the PQR (Welding Performance Qualification Record) is the test report demonstrating the adequacy of that operation; the WPQR is the record certifying that the welder is qualified to perform it.

Three documents to look for in the handover file

  • A valid certificate showing the welder is qualified to EN ISO 9606-1
  • WPS covering the body rings, the conical connection and the support legs
  • The matching PQR test reports and welder certificates

In a workshop without these documents, no matter how clean a seam looks, that joint cannot be reproduced.

3. Full Penetration and Edge Break

Full penetration means the weld metal joins completely through the depth of the base material. A weld that is incomplete at the root still counts as partial penetration even if it looks regular, and it is a crack initiation point on the fusion line.

Why is the edge break (weld run) essential?

  • Chromate coating cannot follow the bead and roughness of the weld area; if a step is left, the coating bridges over it
  • Where the coating bridges, water collects and the steel underneath loses its protection
  • The edge break is the transition region that allows the weld metal to survive temperature changes

4. PT and RT Tests

Seam quality is verified in two stages. PT (liquid penetrant) finds surface-open cracks and porosity; it is fast and economical. RT (radiographic) testing reveals the internal structure of the seam, the root zone and gas cavities; it is expensive but is the only method for critical seams.

When is which needed?

  • Every seam: visual inspection
  • Rough seams and site welds: PT
  • Body rings, conical connections and discharge line welds: PT and RT where required
  • On refurbishment: old seams are cleaned, re-welded and put through the same checks

5. Grinding the Weld Run

If the weld run is not dressed out, a crack starts at the end of the seam and the coating thickens there. That is why every seam is ground at the end and brought flush with the body surface. After grinding, the bead is blended on both sides with a radius and no sharp corner.

Why grinding comes before coating

  • Powder coating and chromate conversion follow the surface geometry one to one
  • At a sharp corner the coating thickness always falls below the target range
  • Bridged coating has to be reworked later, which is a costly cycle

6. Corrosion Starts at the Weld

A rough rule of thumb repeated across the industry is that the large majority of corrosion events requiring maintenance begin not on the flat sheet of a tanker but in the weld and heat-affected areas. The reason is simple: the weld metal has a different chemical composition from the steel, the surface roughness is higher and moisture collects there faster.

Investment in weld quality therefore pays off more than investment in the coating system. A sound weld is the precondition for a sound coating.

7. Cleaning before Chromate Coating

Chromate conversion coating adheres only to a clean surface. Oxide, acid residue, dust and moisture left after welding spoil coating adhesion and the distribution of film thickness.

Sequence of cleaning and control

  1. Weld seams are ground and the beads are given a radius
  2. The surface is acid cleaned and degreased, then dried
  3. It is brought to Sa 2½ by abrasive blasting
  4. A conductivity (soluble salts) measurement is taken and recorded
  5. Chromate conversion, epoxy intermediate coat and 2K polyurethane topcoat are applied
  6. Dry film thickness is measured; any surface outside tolerance is reworked

Weld quality is not a production step but a system: specified by the WPS, proved by the PQR, verified by PT and RT, and prepared for protection by grinding and cleaning. The weakest link in this chain is the one that shortens the life of the tanker most.